Journal of Applied Physics · 1989 · 102 citations · 12 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsInterface ScienceThin FilmsOxide SemiconductorsThin Film AnnealingThin Film Electrical PropertiesThin-film DepositionThin-film MaterialsAnnealing EffectsBreakdown VoltageDielectric ConstantElectrical PropertiesElectrical Properties AnalysisQuartzSiliconTitanium Oxides
Titanium dioxide films of 100–450-nm thickness were deposited on fused quartz and silicon substrates heated at 350 °C by a reactive-ionized cluster-beam deposition. After the deposition, films were annealed at 600 °C in dry O2 ambient. The electrical properties of TiO2 films and the TiO2-Si interface were analyzed. The dielectric constant of the film after the annealing was in a range of 35–108, which depended on the deposition conditions. The films showed a high breakdown voltage and a sufficiently low interface-state density of 1–2×1011 cm−2 eV−1 at the midgap.
12
Ion-beam-assisted deposition of thin films
Peter Martin, H. A. Macleod, R. P. Netterfield et al. · Applied Optics · 1983 · 281 citations
Natural Sciences, Materials Engineering, Materials Science +16