Natural SciencesChemistryMaterials ScienceElectrochemical EngineeringElectrochemistrySurface ChemistryCathode MaterialsChemical OxidationElectrode KineticsElectrode MaterialsSulfur DioxideSulfur OxidesActive SitesAdsorption MechanismsCathodic PolarizationDegradationPerformance DegradationSulfur CathodesSulfur Dioxide ChemistrySulfur Oxides Chemistry
Abstract Sulfur poisoning behavior of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3–δ (LSCF6428) cathode was investigated at T = 1073 K (800 °C) under 0.1 ppm of SO 2 ‐air mixture gas; the amount of supplied SO 2 was controlled by changing the flow rate. Two stages of the performance degradation were found: a rapid degradation at the early stage and a subsequent monotonic degradation. The elemental distributions of SrSO 4 showed a strong correlation between the electrochemically active sites and SrSO 4 reaction sites in the vicinity of the LSCF6428/10GDC interfaces. Considerations were made to attribute the first and the second stages of performance degradation to the SO 2 adsorption and the SrSO 4 formation, respectively. The SO 2 adsorption mechanism was discussed in terms of the high concentration of oxide ion vacancies in the electrochemically active region under the cathodic polarization condition.
13
Sulfur Poisoning of SOFC Cathodes
Yueping Xiong, Katsuhiko Yamaji, Teruhisa Horita et al. · Journal of The Electrochemical Society · 2009 · 88 citations
Natural Sciences, Chemical Engineering, Materials Science +17