Blend Miscibility of Sulfonated Polystyrene Ionomers with Polystyrene:  Effect of Counterion Valency and Neutralization Level

Nancy C. Zhou, Wesley R. Burghardt, Karen I. Winey

Macromolecules · 2007 · 24 citations · 15 references

Concepts

Abstract

Elastic recoil detection (ERD) was used to characterize the phase behavior of blends involving neutralized poly(styrene- ran -styrenesulfonate) ionomers (P(S-SS x )-M) and deuterated polystyrene (dPS). The lightly sulfonated ionomers (acid mole fraction x = 0.007) were neutralized with various cations (M): sodium (Na + ), barium (Ba 2+ ), and zinc (Zn 2+ ). The dPS:P(S-SS 0.007 )-M blends have a higher upper critical solution temperature (UCST) than the dPS:P(S-SS 0.007 ) blends, indicating that neutralizing the acid copolymer reduces blend miscibility. The UCST is higher when P(S-SS 0.007 ) is neutralized (125%) with divalent cations, Ba 2+ and Zn 2+, rather than with a monovalent cation, Na + . In addition, as the level of neutralization increases from 25% to 125%, the miscibility in the dPS:P(S-SS 0.007 )-Zn blends decreases; this was not observed in the dPS:P(S-SS 0.007 )-Na blends. Complementary linear viscoelastic measurements were performed on a copolymer and ionomers with a higher acid content. Upon neutralization, the storage moduli at lower frequencies indicate slower polymer chain relaxations and the self-assembly of ionic functional groups. The specific interactions that produce these physical cross-links also impede blend miscibility.

References

15