X-Ray Photoelectron Spectroscopy of the Fracture Surfaces of Iron/ Epoxy and Titanium/Epoxy Adhesive Joints

F. J. Boerio, D. J. Ondrus

The Journal of Adhesion · 1987 · 14 citations · 6 references

Concepts

Abstract

Abstract The failure path of iron/epoxy and titanium/epoxy lap joints prepared from adherends pretreated with dilute aqueous solutions of ω-aminopropyltriethoxysilane (ω-APS) and then exposed to water at 60°C for varying times was determined using X-ray photoelectron spectroscopy (XPS). Iron/epoxy lap joints prepared using T-APS primers applied at pH 8.0 and tested without exposure to water failed near the oxide/primer interface with only a small amount of adhesive left on the substrate failure surface. Iron/epoxy joints that were primed with T-APS at pH 10.4 and tested without immersion in water failed partly within the adhesive and partly near the interface. All of the iron/epoxy joints failed in the primer near the primer/oxide interface when tested after exposure to water for seven days but very little corrosion of the substrates was observed. When titanium/epoxy lap joints were tested without exposure to water, failure was partly within the adhesive and partly near the primer/oxide interface regardless of the pH at which the primer was applied. However, the failure path shifted to near the primer/oxide interface after the joints were immersed in water for seven days. It was concluded that failure of the joints after exposure to water was associated with hydrolysis within the primer rather than with extensive corrosion of the substrate.

References

6