Natural SciencesChemical EngineeringChemistryOrganic ChemistryPolymer ChemistryPolymer EngineeringOrganic Waste RecoveryPolymer AnalysisPolymer CharacterizationPolymer ProcessingWaste CharacterizationAromatic HydrocarbonsHydrolysisHydrolysis Of Waste PolymersHydrolysis ReactionsOrganic Waste ConversionPolymer PyrolysisPolymer Waste CharacterizationPyrolysis
Abstract Poly(vinyl chloride) PVC pyrolysis and hydrolysis are conducted in a fixed bed reactor and in an autoclave, respectively, under different operating conditions such as the temperature and time. The product distribution is studied. For the PVC pyrolysis process, the main gas product is HCl (55% at 340°C), there is 9% hydrocarbon gas (C 1 –C 5 ), the liquid product fraction is about 5% (at 340°C), and the solid residue fraction is about 31% (at 340°C). For the hydrolysis process, the main gas product is HCl (55.8% at 240°C) and the solid residue is about 49.6% (at 240°C). The pyrolysis liquid product is analyzed by using gas chromatography with magic‐angle spinning. Aromatic hydrocarbons are the main class (90%), of which the major part is benzene (33%). The residue produced through pyrolysis and hydrolysis is investigated by high‐resolution solid‐state 13 C‐NMR. These details revealed by the high‐field NMR spectra provide importmant information about the chemical changes in the PVC pyrolysis and hydrolysis process. The mechanism of PVC hydrolysis dechlorination is also discussed. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 90: 3252–3259, 2003
11
Study of the Low Temperature Pyrolysis of PVC
Shibai Ma, Jun Lu, Jinsheng Gao · Energy & Fuels · 2002 · 139 citations