Effects of Additives on the Densification and Microwave Dielectric Properties of Binary CaO–B<sub>2</sub>O<sub>3</sub>–SiO<sub>2</sub> Glass

Sea‐Fue Wang, Chuang-Chung Chiang, Yuh‐Ruey Wang, Yung‐Fu Hsu

Japanese Journal of Applied Physics · 2010 · 12 citations · 13 references

Concepts

Abstract

Glass systems, consisting of binary CaO–B 2 O 3 –SiO 2 (CBS) glass (referred to as glass AB) and various amounts of Li 2 CO 3 , TiO 2 , and Al 2 O 3 additives, were prepared in this study. The effects of the additives on the densification and microwave dielectric properties of binary CBS glass were investigated. Binary glass AB was not densified until the sintering temperature reached 875 °C; however, with the addition of 1 wt % Li 2 CO 3 (referred to as glass L1), the glass achieved a maximum density at 825 °C. The resultant glass-ceramics contained a major phase quartz, SiO 2 , and a minor phase, CaB 2 O 4 , and had a dielectric constant ( ε r ) varying from 4.10 to 4.23 and a minimum tan δ of 0.0015, as frequency increased from 4.3 to 18.6 GHz. For glass L1 with further addition of the ceramic filler Al 2 O 3 (up to 30 wt %), the maximum densification was reached at 775 °C and the formation of CaB 2 O 3 and SiO 2 crystallites was suppressed. Both ε r and tan δ increased with the Al 2 O 3 content of the glass-ceramics. Further addition of the crystallization agent TiO 2 (up to 5 wt %) to glass L1 slightly reduced the sintering temperature to 800 °C. The X-ray diffraction (XRD) intensities of the quartz SiO 2 and CaB 2 O 4 crystallites as well as the ε r and tan δ values of the resultant glass-ceramic increased with the amount of TiO 2 added.

References

13