Dental Materials Journal · 2013 · 14 citations · 11 references
DentistryDental Materials ScienceCeramic MaterialsCeramicsDental MaterialsDental CeramicsDenture Base MaterialsCeramic Dental MaterialsCeramic Material PropertiesFlexural StrengthFlexural Strength TestingHardnessHardness Of Dental CeramicsZirconiaZirconia Materials
Plate-like specimens were prepared, using a diamond saw, from Cercon -a pre-sintered yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) block. These specimens were treated with 10 kinds of dental materials which acted as contaminants, and then sintered at 1,350°C or 1,450°C. After the final firing, specimens were subjected to a three-point flexural test and Vickers hardness test. Their surfaces were also characterized by scanning electron microscopy and X-ray diffractometry. Phosphorus-containing contaminants reduced the three-point flexural strength and hardness of final sintered zirconia due to the formation of YPO4 and phase transformation from tetragonal to monoclinic zirconia. Gypsum also reduced both mechanical properties due to the formation of CaZrO3 and phase transformation from tetragonal to cubic zirconia. Other contaminants showed no adverse effects on the mechanical properties of final sintered zirconia.
11
Seiji Ban, H. Sato, Y. Suehiro et al. · Journal of Biomedical Materials Research Part B Applied Biomaterials · 2008 · 180 citations
Dentistry, Dental Materials Science, Restorative Dentistry +17