Electrical properties of four anisotropically conductive adhesives were characterised. The effect of bonding temperature as well as 60°C/95% RH-test on contact resistance values of the adhesive joints was studied. The resistivities of the adhesive joints were measured as a function of temperature. In addition, the joint microstructures were examined with optical and the scanning electron microscopy and wetting properties of the solder alloys were measured with the wetting balance method. Regardless of the adhesive, the average contact resistance values were on the same level but the standard deviation was considerably higher with Au/Ni-coated conductors than with bare copper conductors. In the hot and humid environment test the best results were achieved with tin-bismuth and tin-bismuth-zinc-filled adhesives on bare copper conductors. On the contrary, joints produced with Au/Ni-coated conductors failed in this test. It is likely that the poor performance of the Au/Ni-coated circuits results from the strong oxidation of nickel in the presence of moisture. The small exposed area and anodic electrochemical potential of nickel compared with the large area of noble gold accelerates this reaction.