Defect properties of implanted boron in ZnSe

Bernd Ittermann, G. Welker, F. Kroll, K. Marbach, David A. Peters

Physical review. B, Condensed matter · 1999 · 22 citations · 54 references

Concepts

Abstract

Microscopic properties of B in ZnSe are investigated by means of $\ensuremath{\beta}$-radiation-detected nuclear magnetic resonance $(\ensuremath{\beta}$-NMR). After implantation of spin-polarized, radioactive ${}^{12}\mathrm{B}$ nuclei in nominally undoped ZnSe single crystals at stationary concentrations of $\ensuremath{\sim}{10}^{8} {\mathrm{cm}}^{\ensuremath{-}3},$ three different B-defect configurations can be distinguished. First, an unperturbed fraction at cubic lattice sites, identified as substitutional ${\mathrm{B}}_{\mathrm{Zn}}^{+}$ by a dipolar linewidth analysis. Second, a smaller part of ``perturbed'' probes attributed also to ${\mathrm{B}}_{\mathrm{Zn}}^{+}$ but with nearby Se vacancies. And third, a paramagnetic configuration, tentatively assigned to the isolated interstitial ${\mathrm{B}}_{i}^{2+}.$ Temperature-dependent measurements show a conversion of ${\mathrm{B}}_{i}$ to ${\mathrm{B}}_{\mathrm{Zn}}$ with an activation energy of ${E}_{a}=0.61(3) \mathrm{eV}$ which we attribute to ${\mathrm{B}}_{i}$ migration. After this annealing stage we find a ${\mathrm{B}}_{\mathrm{Zn}}$ fraction of about 85%, i.e., an excellent ``doping efficiency.'' A substantial inward relaxation of the nearest Se and next-nearest Zn atoms around the ${\mathrm{B}}_{\mathrm{Zn}}^{+}$ donor is observed and compared with model predictions.

References

54