Chemical Vapor Deposition · 2004 · 28 citations · 20 references
Natural SciencesMaterials EngineeringMaterials ScienceInorganic ChemistryOptical MaterialsSurface SciencePhotocatalysisPhotochemical SynthesisPhotochemistryThin Film OxidationAtmospheric PressurePhotocatalytic MaterialsPhotocatalytic OxidationPhotocatalytic TreatmentPhotochemical Oxidation
Coatings of yellow γ‐WO 3 are deposited on glass by APCVD of WOCl 4 and either ethanol or ethylacetate at 350–450°C. The yellow films show significant photoactivity for the destruction of stearic acid, and photoinduced superhydrophilicity. Preparation of blue reduced WO 2.92 films from the same reaction at higher substrate temperatures of 500–600 °C (Figure) is also found to be possible. These films show no photoactivity, but can be converted into the fully stoichiometric photoactive form simply by heating in air.
20