Journal of Physics C Solid State Physics · 1980 · 19 citations · 5 references
Natural SciencesChemistryPhysicsCondensed Matter PhysicsSolid-state ChemistrySpectroscopyMagnetic Properties Of SolidsPhase ChangePhase TransitionsRelaxation MechanismsSolid-state Phase TransitionsFerroelectric Phase TransitionsLongitudinal RelaxationProton RelaxationRelaxation In SolidsRelaxation Time MeasurementsSpin RelaxationSpin Relaxation MechanismsSpin-lattice Relaxation
Lithium ammonium sulphate (LAS) undergoes a phase transition at TC1=459.5K from a paraelectric phase (phase I) to a ferroelectric phase (phase II) and again at TC2=283K to a polar ferroelastic phase (phase III). Proton spin lattice relaxation time measured at 10 MHz in powdered LAS in the temperature range 480 to 77K shows discontinuous changes at the two transitions.
5
Ferroelectricity in NH<sub>4</sub>LiSO<sub>4</sub>
Toshiharu Mitsui, Tateki Oka, Y. Shiroishi et al. · Journal of the Physical Society of Japan · 1975 · 141 citations