Thermoelectric Properties of Y-Doped Polycrystalline SrTiO<sub>3</sub>

H. Obara, Atsushi Yamamoto, Chul‐Ho Lee, Keizo Kobayashi, Akihiro Matsumoto, Ryoji Funahashi

Japanese Journal of Applied Physics · 2004 · 101 citations · 7 references

Concepts

Abstract

The thermoelectric properties of Y-doped polycrystalline SrTiO 3 (Sr 1- x Y x TiO 3 ) are measured from 10 K to 900 K. The Y component is doped up to the solubility limit of Sr 1- x Y x TiO 3 , x =0.1. The Y-doped polycrystalline samples show a low resistivity, ∼1 ×10 -5 Ω·m and a large absolute value of the Seebeck coefficient, ∼150 µV/K, at room temperature. Consequently, they have a high power factor, 1.2 ×10 -3 W/mK 2 , defined as PF = S 2 /ρ, where S is the Seebeck coefficient and ρ is the resistivity. Furthermore, we observe a decrease in the thermal conductivity of SrTiO 3 due to phonon scattering by the Y dopant.