Journal of The Electrochemical Society · 1965 · 21 citations · 0 references
Natural SciencesChemistryMaterials SciencePhysical ChemistrySurface ChemistrySurface ScienceCrystal ChemistryCrystallographySurface Chemistry Of SolidsSurface KineticsSurface MorphologySurface OxidationCrystal MorphologyCrystal Plane OrientationCrystal Surface MorphologyImpuritiesSurface Chemistry Of OxidationSurface Oxidation MechanismsSurface Oxidation StatesTungsten-based Materials
The oxidation of tungsten above 1800°C is described in terms of deviations from gas collision theory (Hertz‐Knudsen equation). The probability that a colliding oxygen molecule will react with tungsten is strongly dependent on crystal orientation. Of the crystal faces examined, (100) surfaces oxidize most rapidly with a reaction probability of 0.4. (111) and (110) surfaces oxidize at approximately the same rate as polycrystalline tungsten. The morphology of oxidized (100) surfaces is smooth with the exception of occasional stepped octahedral pyramids each bound by {111} faces. The morphology of (111) surfaces is smooth except for numerous stepped tetrahedral pyramids each bound by {100} faces. Initiation of these shapes is not associated with dislocations or detectable impurities. However, dislocations subsequently cluster at mature octahedral pyramids. The morphology of oxidized (110) tungsten surfaces consists of extremely irregular surfaces and macroscopic ledges, but shapes clearly related to crystal geometry were not identified.