Gelation Process and Phase Separation of PVA Solutions As Studied by a Light Scattering Technique

H. Takeshita, Toshiji Kanaya, Koji Nishida, Koichi Kaji

Macromolecules · 1999 · 77 citations · 8 references

Concepts

Abstract

Time-resolved light scattering measurements were performed on gelation processes of poly(vinyl alcohol) (PVA) solutions at 25 °C in mixtures of dimethyl sulfoxide (DMSO) and water (H 2 O) with volume ratios of 60/40 and 80/20. It was found that the scattering profile I ( Q ) from a 60/40 (DMSO/H 2 O) solution has a maximum whose position Q m is independent of time and that the intensity I ( Q ) at Q = Q m increases exponentially with time. These observations agree with the theoretical predictions for the initial stage of spinodal decomposition (SD) type phase separation, while the scattering profile I ( Q ) from a 80/20 solution has no peak. It is therefore concluded that the SD type microphase separation occurs before gelation in the 60/40 solution, but not in the 80/20 solution. On the basis of present, as well as past results, a possible mechanism of the gelation process for PVA solutions has been proposed.

References

8