Applied Physics Letters · 1988 · 18 citations · 7 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMaterials ChemistrySolid-state ChemistryMagnetic OxidesMagnetic Properties Of SolidsMagnetic Recording MaterialsMagnetism In SolidsMagneto-optic MaterialsThin Film Magnetic PropertiesCoolingDoping MechanismsFast PyrolysisMagneto-optic Recording MaterialsMagneto-optical Recording MediaPyrolysisRapid CoolingYttrium Iron Garnet
Al-doped Bi-Dy iron garnet films have been fabricated by the pyrolysis method on glass substrates, and the effects of Ba doping and rapid cooling on the coercivity (Hc) were investigated. Films were quenched from 660 °C to room temperature within about 120 s. Rapid cooling causes a rise of Hc, and a small amount of Ba doping enhances this effect. Hc values near 4200 Oe at room temperature were obtained in rapidly cooled films with the composition Bi1Dy1.96Ba0.04Fe4.4Al0.6O12.
7