Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsThin FilmsCoatingsDielectric MaterialsDielectricsFerroelectric MaterialsInorganic MaterialsThin-film MaterialsCeramic DielectricsDielectric ConstantFerroelectric Thin FilmsFilm ThicknessOxide DielectricsThin Film FerroelectricsThin Oxide FilmsThin-film Dielectrics
Ferroelectric Pb(Zr,Ti)O 3 (PZT) heterolayered thin films were fabricated by the alkoxide-based sol–gel method. PZT (20/80) and PZT (80/20) stock solutions were made and alternately spin-coated on the Pt/Ti/SiO 2 /Si substrate. Each layer was dried at 300°C for 30 min and sintered at 650°C for 1 h. The coating and heating procedure was repeated 6 times to form heterolayered films. PZT film thickness, obtained by one cycle of drying/sintering, was approximately 80 nm. The PZT heterolayered films showed dense and fine grain structures with a grain size of less than 0.2 µm. The relative dielectric constant and the dielectric loss of the 6-coated PZT heterolayered film(PZT-6) were approximately 1385 and 3.3%, respectively. As the number of coatings increased, remanent polarization increased, the coercive field decreased and the values for the PZT-6 film were 8.13 µC/cm 2 and 12.5 kV/cm, respectively. The leakage current density of the PZT-6 film at 5 V was 8.8 ×10 -13 A/cm 2 .
10
Isaku Kanno, Shigenori Hayashi, Takeshi Kamada et al. · Japanese Journal of Applied Physics · 1993 · 71 citations
Natural Sciences, Materials Engineering, Materials Science +17