The evolution of microstructure and photoluminescence of SiCN films with annealing temperature

Xi‐Wen Du, Yang Fu, Jing Sun, Pei Yao

Journal of Applied Physics · 2006 · 24 citations · 25 references

Concepts

Abstract

Silicon carbonitride (SiCN) films were deposited by radio-frequency magnetron sputtering and then annealed at different temperatures from 1100to1300°C in hydrogen atmosphere. The as-deposited films and films annealed at 1100°C did not show photoluminescence (PL), whereas strong PL peaks appeared at 355 and 469nm after annealing at 1200 and 1300°C. X-ray diffraction, transmission electron microscope, and Fourier transform infrared spectrometer results show that the enhancement of PL properties is due to the change of microstructure and composition.

References

25