Journal of Applied Polymer Science · 2001 · 52 citations · 19 references
Natural SciencesBiochemistryChemistryPolymer ChemistryPolymer MaterialsThermal AnalysisCalorimetryPolymer CharacterizationPolymer DegradationPolymer Physical ChemistryThermal Properties Of MaterialsThermogravimetric AnalysisPolymer Thermal DegradationThermal Degradation ProductsThermal Degradation StudiesThermal PropertiesThermal Stability Of PolymersThermally Stable PolymersWeight Loss Measurement
Abstract Thermal analyses of poly(3‐hydroxybutyrate) (PHB), poly(3‐hydroxybutyrate‐ co ‐3‐hydroxyvalerate) [P(HB–HV)], and poly(3‐hydroxybutyrate‐ co ‐3‐hydroxyhexanoate) [P(HB–HHx)] were made with thermogravimetry and differential scanning calorimetry (DSC). In the thermal degradation of PHB, the onset of weight loss occurred at the temperature (°C) given by T o = 0.75 B + 311, where B represents the heating rate (°C/min). The temperature at which the weight‐loss rate was at a maximum was T p = 0.91 B + 320, and the temperature at which degradation was completed was T f = 1.00 B + 325. In the thermal degradation of P(HB–HV) (70:30), T o = 0.96 B + 308, T p = 0.99 B + 320, and T f = 1.09 B + 325. In the thermal degradation of P(HB–HHx) (85:15), T o = 1.11 B + 305, T p = 1.10 B + 319, and T f = 1.16 B + 325. The derivative thermogravimetry curves of PHB, P(HB–HV), and P(HB–HHx) confirmed only one weight‐loss step change. The incorporation of 30 mol % 3‐hydroxyvalerate (HV) and 15 mol % 3‐hydroxyhexanoate (HHx) components into the polyester increased the various thermal temperatures T o , T p , and T f relative to those of PHB by 3–12°C (measured at B = 40°C/min). DSC measurements showed that the incorporation of HV and HHx decreased the melting temperature relative to that of PHB by 70°C. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 82: 90–98, 2001
19
Isodimorphism in bacterial poly(β-hydroxybutyrate-co-β-hydroxyvalerate)
Terry L. Bluhm, Gordon K. Hamer, R. H. Marchessault et al. · Macromolecules · 1986 · 388 citations