ACS Nano · 2008 · 25 citations · 49 references
Natural SciencesMaterials EngineeringMaterials SciencePolymer ChemistryPolymer MaterialsThin FilmsCreep BehaviorCreep DeformationPolymer PhysicsPolymer Thin FilmsStress RelaxationStress-strain BehaviorCreep Of Polymer MaterialsPolymer CreepPolymer ViscoelasticityStress Deformation BehaviorStress Relaxation Of PolymersStress-strain AnalysisStress-strain CurveStress-strain Relations
This paper investigates molecular-scale polymer mechanical deformation during large-strain squeeze flow of polystyrene (PS) films, where the squeeze flow gap is close to the polymer radius of gyration (R(g)). Stress-strain and creep relations were measured during flat punch indentation from an initial film thickness of 170 nm to a residual film thickness of 10 nm in the PS films, varying molecular weight (M(w)) and deformation stress rate by over 2 orders of magnitude while temperatures ranged from 20 to 125 degrees C. In stress-strain curves exhibiting an elastic-to-plastic yield-like knee, the response was independent of M(w), as expected from bulk theory for glassy polymers. At high temperatures and long times sufficient to extinguish the yield-knee, the mechanical response M(w) degeneracy was broken, but no molecular confinement effects were observed during thinning. Creep measurements in films of 44K M(w) were well-approximated by bulk Newtonian no-slip flow predictions. For extrusions down to a film thickness of 10 nm, the mechanical relaxation in these polymer films scaled with temperature similar to Williams-Landel-Ferry scaling in bulk polymer. Films of 9000K M(w), extruded from an initial film thickness of 2R(g) to a residual film thickness of 0.5R(g), while showing stress-strain viscoelastic response similar to that of films of 900K M(w), suggestive of shear-thinning behavior, could not be matched to a constitutive flow model. In general, loading rate and magnitude influenced subsequent creep extrusion depth of high-M(w) films, with deeper final extrusions for high loading rates than for low loading rates. The measurements suggest that, for high-resolution nanoimprint lithography, mold flash or final residual film thickness can be reduced for high strain and strain rate loading of high-M(w) thin films.
49
Hardness measurement at penetration depths as small as 20 nm
J. B. Pethicai, R. Hutchings, W. C. Oliver · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · 1983 · 924 citations
Natural Sciences, Materials Engineering, Materials Science +17