With micro-Raman spectroscopy and x-ray diffraction (XRD), we studied ZnO crystals implanted with Mn, Fe, Co, and Ni, respectively, with implantation concentrations from 4 up to 16 at. %. Using thermal treatments in air up to 700 °C, we analyzed the annealing effect on the ZnO crystal lattice as well as the onset of secondary phases and their microstructure on the sample surface. While the 500 °C treatment induces a considerable annealing, secondary phases are observed for transition metal (TM) concentrations ≥8 at. % after the treatment at 700 °C. Their microstructure strongly depends on the TM species. Various stoichiometric and nonstoichiometric TM oxide precipitates as well as elemental TM clusters are identified by their Raman and XRD signatures and their possible magnetic impact is discussed.