Silica capping for Al0.3Ga0.7As/GaAs and In0.2Ga0.8As/GaAs quantum well intermixing

G. Li, S. J. Chua, Shijie Xu, X. C. Wang, Amr S. Helmy, Maolong Ke, J.H. Marsh

Applied Physics Letters · 1998 · 29 citations · 12 references

Concepts

Abstract

Spin-on silica capping has been demonstrated to be an effective dielectric encapsulant layer for quantum well (QW) intermixing at temperatures significantly lower than for conventionally deposited silica. A blueshift of up to 125 meV was observed in the photoluminescence (PL) peak energy of both GaAs and InGaAs QWs after annealing for less than 60 s at 850 °C, without noticeable degradation in the PL emission intensity. A threshold temperature was identified below which no significant QW disordering took place. The activation energy for Al diffusion in Al0.3Ga0.7As/GaAs QWs was about 2.55 eV. Broadly similar effects were seen for In0.2Ga0.8As/GaAs QWs but, in addition, strain effects appear to enhance disordering during the early stages of the anneal.

References

12