Semiconductor Science and Technology · 1993 · 55 citations · 13 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsInorganic ChemistryPhysical ChemistryDefect ThermodynamicsHydrogen AtomRadiation Damage In MaterialsSemiconductor DefectsSilicon MaterialsThermal Properties Of SemiconductorsElectron Beam Irradiation EffectsHydrogen Content AnalysisSecondary Ion Mass SpectrometrySilicon ChemistrySilicon DefectsSilicon ImpuritiesSolubility
Boron-doped silicon ((B) approximately 1017 cm-3) was heated in H2 gas at a temperature in the range 900<or=T<or=1300 degrees C and quenched to room temperature. Some of the dissolved hydrogen formed H-B pairs and the remainder (Hh), which was infrared inactive was released during anneals at T<or=200 degrees C leading to an increase in (H-B). The total hydrogen content, consistent with secondary-ion mass spectrometry, yielded a solubility given by SH=9.1*1021 exp(-1.80 eV/kT) cm-3. 2 MeV electron irradiation at room temperature converted Hh into defects incorporating two hydrogen atoms, suggesting that Hh may be present as H2 molecules.
13
Defects in single-crystal silicon induced by hydrogenation
N. Johnson, F. A. Ponce, R. A. Street et al. · Physical review. B, Condensed matter · 1987 · 451 citations