Mass transfer and doping during electrolyte-plasma treatment of cast iron

A.D. Pogrebnjak, O. P. Kul’ment’eva, A.P. Kobzev, Yu. N. Tyurin, S. I. Golovenko, A. G. Boiko

Technical Physics Letters · 2003 · 27 citations · 2 references

Concepts

Abstract

The surface and subsurface layers of cast iron articles upon electrolyte-plasma treatment (EPT) were studied for the first time by a combination of methods, including Rutherford backscattering, elastic recoil detection analysis, X-ray diffraction, optical metallography, and microhardness measurements. It was found that tungsten and copper ions are incorporated into the surface layers of the metal. Total thickness of an EPT-hardened layer is about 3 mm, the maximum hardness (up to 7000 MPa) being observed at a depth from 1 to 2.5 mm. The X-ray diffraction analysis (i) shows that the EPT-hardened layer comprises a mixture of α and γ phases, (ii) indicates the formation of a fine-grained martensite structure with high dislocation density (above 10 12 cm −2 ) and an oxide (FeO) phase, and (iii) reveals mass transfer involving the doping elements (W and Cu).

References

2