Electrochemical and Solid-State Letters · 2003 · 65 citations · 13 references
Natural SciencesMaterials EngineeringMaterials ScienceElectrochemistryMagnetic MaterialsThin FilmsElectrode MaterialsFerromagnetic MaterialsFerromagnetismMagnetic Thin FilmsThin Film Magnetic PropertiesThin Film OxidationFerrite Thin FilmsFerrous AlloysMagnetic FluxMagnetic Flux DensityPlatingSoft Ferromagnetic MaterialsSoft Magnetic Thin FilmsThin-film Magnetic Materials
A CoFe binary alloy film with 24 kG of saturation magnetic flux density, was prepared by electrodeposition. The value of the CoFe alloy film prepared by electrodeposition from the conventional bath is usually equal to 21 kG. With the addition of trimethylamineborane, a well-known reducing agent, the value was found to increase to 23 kG. Furthermore, with the use of a separated compartment dual cell system, a value as high as 24 kG was reached. For obtaining the highest it was found to be essential to avoid the oxidation of ferrous ion to ferric ion in the plating bath. The coercivity, values were 15, 14, and 15 Oe for the films with 20, 23, and 24 kG of respectively. The key for obtaining high materials is to avoid the oxidation of ferrous ions in the bath. In addition, it was found that the value of 15 Oe for CoFe film with the highest value of 24 kG could be lowered to 8 Oe by annealing in an applied magnetic field of 500 Oe. © 2003 The Electrochemical Society. All rights reserved.
13
Properties of a new soft magnetic material
S. X. Wang, Nian X. Sun, Masahiro Yamaguchi et al. · Nature · 2000 · 303 citations