Natural SciencesMaterials EngineeringMaterials ScienceBiomaterialsMaterials CharacterizationMechanical Behavior Of MaterialsComposite MaterialsComposite ResinsCompressive PropertiesDental CompositesNanocompositesStrength PropertiesCompressive StrengthCompressive Strength TestingFillers Effects On Compressive StrengthMechanical Properties Of NanocompositesNanocomposite MaterialsRepeated Measures AnovaResin Compressive StrengthResin Nanoceramics
AIM: The purpose of the study is to assess and compare compressive strength of newer nanocomposites (FiltekZ350, Ceram X Mono, Ceram X Duo) with microhybrid (Tetric Ceram) and to compare difference in compressive strength of newer nanocomposites. MATERIALS AND METHODS: Forty eight specimens of composite were fabricated using customized biparpite brass mold measuring 5mm x 5mm and were grouped with twelve specimens in each Group I : Tetric Ceram, Group II: Filtek Z 350, Group III : Ceram X Mono, Group IV : Ceram X Duo. Composite resins are placed in cylindrical recesses and covered with mylar strip and are cured using QHL light curing unit. Compressive strength is evaluated using Instron machine. Results are statistically analyzed using One way Anova and Student t test. Analysis demonstrated that nanocomposites have better compressive strength than micro hybrid (P<0.001). RESULTS: Within the limitations of the study, it can be concluded that nanocomposites have better compressive strength than microhybrid composite and nanocomposite showed optimal compressive strength of 312 - 417 Mpa.
1
Eduardo Gonçalves Mota, Hugo Mitsuo Silva Oshima, Luiz Henrique Burnett et al. · PubMed · 2006 · 40 citations
Dentistry, Dental Biomaterials Science, Dental Materials Science +17