Sensitization behaviour of 11-12% Cr AISI 409 stainless steel during low heat input welding

Cornelis Janise Van Niekerk, Madeleine Du Toit

Research Online (University of Wollongong) · 2011 · 13 citations · 6 references

Full text

Open access

Concepts

Abstract

The study comprised of the investigation into the sensitization
\ncharacteristics of AISI 409 titanium stabilized ferritic stainless steel
\nduring low heat input welding. AISI 409 is a fully ferritic stainless
\nsteel used in catalytic converters and tubing for automotive exhaust
\nsystems due to the supposition that sensitization does not occur
\nduring low heat input welding. Two plates of 2 and 4 mm were
\ntested for sensitization during low heat input welding. The study
\nconfirmed that chromium carbide (M23C6) precipitation occurs on
\nthe grain boundaries in the heat-affected zone with consequent
\ndepletion of Cr adjacent to the grain boundaries during welding. In
\nthe 2 mm plate sensitization occurred in the heat input range of 0.1
\nkJ/mm to above 0.25 kJ/mm and in the 4 mm plate sensitization
\noccurred in the heat input range of 0.2 to 0.9 kJ/mm. Ti stabilization
\nis ineffective at the heat inputs used in this investigation due to the
\nrapid cooling rate through the temperature region where TiC precipitates.
\nThe presence of N was found to be detrimental since it
\nconsumes Ti on cooling, forming TiN, effectively lowering the
\namount of Ti available for TiC formation during rapid cooling after
\nwelding. Annealing for 5 minutes at 725°C does not improve the
\nsensitization characteristics of the welded plate. There is a linear
\nincrease in grain size as heat input increases. The resistance to
\npitting corrosion decreases in the sensitized, welded plate in the
\nheat-affected zone adjacent to the fusion line of welding.

References

6