Grain Size Dependence of Hardness in Dense Submicrometer Alumina

Andreas Krell, Paul S. Blank

Journal of the American Ceramic Society · 1995 · 233 citations · 10 references

Concepts

Abstract

Pressureless sintered alumina compacts with a submicrometer microstructure exhibit a hardness that approaches or even exceeds the level of advanced hotpressed composites of Al 2 O 3 + 35 vol% TiC, whereas the strength of both ceramics is approximately the same. The combination of reduced dislocation mobility (due to the small grain size), high density, and density homogeneity are the prerequisites for the surprisingly high hardness. Quasiconventional powder processing is used to produce these outstanding alumina bodies.

References

10