Analysis of Crystallite Size and Lattice Deformations Changes in an Oxide Layer on P91 Steel / Analiza Zmian Wielkosci Krystalitów I Odkształcen Sieciowych W Warstwie Tlenków Na Stali P91

M. Gwoździk, Z. Nitkiewicz

Archives of Metallurgy and Materials · 2013 · 12 citations · 0 references

DOIFull text

Open access

Concepts

Abstract

The paper contains results of studies on X-ray diffraction analysis XRD (studying the phase composition, crystallite sizes and lattice deformations) of oxide layers on P91 steel, operated for a long time at an elevated temperature (T = 535°C, t = 70,000 h). X-ray studies were carried out on the inner surface of a tube, and then the layer surface was polished down to 3.5 μm and the diffraction measurements were performed again to determine individual oxide layers. It has been found that a three-zone oxide layer is formed as a result of long-term operation of P91 steel at the temperature of 535°C. Hematite occurs on the inner surface of the tube. Then magnetite appears below hematite. Going deeper into the layer there is a spinel, i.e. a mixture of magnetite and chromite. A visible decay of total intensity for Fe 2 O 3 is observed already at the polishing depth of 3.5 μm. In the case of Fe 3 O 4 and FeCr 2 O 4 an increase in total intensity is observed already from 7 μm, what manifests in narrowing the diffraction line and hence in increasing the crystallites size and in the relaxation of stresses in this oxide layer. The broadening of a diffraction line caused by a small size of crystallites is expressed by the Scherrer relationship. Instead, the β 2 broadening resulting from lattice distortions (relaxation of stresses) was determined from the Taylor relationship.