Third-Order Elastic Constants of Tin and of a Tin-Indium Alloy

K. D. Swartz, Wei-Jing Chua, C. Elbaum

Physical review. B, Solid state · 1972 · 25 citations · 6 references

Concepts

Abstract

The complete set of 12 third-order elastic constants (TOEC) of white (metallic) tin and a set of 11 of the 12 TOEC of tin containing 0.3 at.% indium were determined from the hydrostatic and uniaxial stress dependence of ultrasonic velocity. The experiments were carried out on single crystals, using the two-specimen interferometric method of measuring velocity changes. In both the pure and the alloyed crystals ${c}_{333}$ was largest and negative, and only ${c}_{123}$ was positive. Some of the TOEC for the alloy were found to differ from the corresponding ones for the pure tin by as much as 20%, e.g. (in units of ${10}^{12}$ dyn/${\mathrm{cm}}^{2}$), ${c}_{112(\mathrm{tin})}=\ensuremath{-}5.83\ifmmode\pm\else\textpm\fi{}0.12$ and ${c}_{112(\mathrm{alloy})}=\ensuremath{-}4.82\ifmmode\pm\else\textpm\fi{}0.13$. All the second-order elastic constants were measured for both types of specimens and were found to be the same within the experimental uncertainty of \ensuremath{\approx} 0.1%.

References

6