Publication | Closed Access
Improved initial drop in operational lifetime of blue phosphorescent organic light emitting device fabricated under ultra high vacuum condition
66
Citations
13
References
2011
Year
Optical MaterialsEngineeringLuminance LossOptoelectronic DevicesHv Device EmlLuminescence PropertyPhosphorescence ImagingElectronic DevicesOptical PropertiesInitial Luminance DropInitial DropElectrical EngineeringOptoelectronic MaterialsNew Lighting TechnologyOperational LifetimeWhite OledSolid-state LightingApplied PhysicsOptoelectronicsPhosphorescence
A blue phosphorescent organic light emitting device fabricated under the ultra high vacuum (UHV) condition of 6.5 × 10−7 Pa decreases the initial luminance drop upon lifetesting under a constant dc current of 15 mA/cm2 by 3 times compared to a device fabricated under a high vacuum (HV) condition of 7.6 × 10−6 Pa resulting in a 23% increase in half lifetime. We calculate a water content of 10−4 mol. % in the UHV device emissive layer (EML) and 10−2 mol. % in the HV device EML. We discuss the effects of water on luminance loss and voltage rise for the devices.
| Year | Citations | |
|---|---|---|
Page 1
Page 1