Dalton Transactions · 2015 · 45 citations · 36 references
Natural SciencesMaterials EngineeringMaterials ScienceCrystal StructureInorganic ChemistryMagnetic MaterialsAntiferromagnetismMagnetic OxidesMagnetic Properties Of SolidsMagnetic SusceptibilityMagnetism In SolidsPerovskite MaterialsAntiferromagnetic OrderingMagnetic PropertiesMagnetic Sublattice StructurePerovskite Crystal StructurePowder DiffractionPowder Diffraction AnalysisPowder Neutron DiffractionUnit Cell Parameters
The perovskite polymorph of Mn(2)CrSbO(6) compound has been synthesized at 8 GPa and 1473 K. It crystallizes in the monoclinic P21/n space group with cell parameters a = 5.2180 (2) Å, b = 5.3710(2) Å, c = 7.5874(1) Å and β = 90.36(1)°. Magnetic susceptibility and magnetization measurements show the simultaneous antiferromagnetic ordering of Mn(2+) and Cr(3+) sublattices below TN = 55 K with a small canting. Low temperature powder neutron diffraction reveals a commensurate magnetic structure with spins confined to the ac-plane and a propagation vector κ = [1/2 0 1/2]. The thermal treatment of this compound induces an irreversible phase transition to the ilmenite polymorph, which has been isolated at 973 K and crystallizes in R3[combining macron] space group with cell parameters a = 5.2084 (4) Å and c = 14.4000 (11) Å. Magnetic susceptibility, magnetization and powder neutron diffraction data confirm the antiferromagnetic helical ordering of spins in an incommensurate magnetic structure with κ = [00 0.46] below 60 K, and the temperature dependence of the propagation vector up to κ = [00 0.54] at about 10 K.
36
Physics and Applications of Bismuth Ferrite
Gustau Catalán, J. F. Scott · Advanced Materials · 2009 · 4.2K citations
Yoshinori Tokura, S. Seki, Naoto Nagaosa · Reports on Progress in Physics · 2014 · 966 citations