Journal of Biomedical Materials Research Part A · 2010 · 411 citations · 27 references
EngineeringBioengineeringBiomedical EngineeringBiocompatibilityBiomaterialsTissue EngineeringBioactive GlassesBioceramicsBone TissueBone Tissue EngineeringScaffold FabricationTissue Engineering ScaffoldsBone Graft ScaffoldsBone Regeneration ScaffoldsBone RepairGlass CompositionHydroxyapatite ScaffoldsScaffold-based Bone RepairSilicate Bioactive GlassesSubcutaneous Implantation Testing
Bioactive glass scaffolds mimicking trabecular bone microstructure were evaluated for bone repair applications. This study reports scaffold preparation and examines how glass composition influences degradation and hydroxyapatite conversion in simulated body fluid. Scaffolds (78–82 % porosity, 100–500 µm pores) were fabricated by polymer foam replication from silicate, borosilicate, or borate glasses, and their in‑vitro osteogenic response and in‑vivo rat subcutaneous implantation were evaluated. Higher B₂O₃ content accelerated hydroxyapatite conversion and raised solution pH, while also reducing compressive strength over time, demonstrating that varying SiO₂/B₂O₃ ratios tunes bioactivity and degradation.
Bioactive glass scaffolds with a microstructure similar to that of dry human trabecular bone but with three different compositions were evaluated for potential applications in bone repair. The preparation of the scaffolds and the effect of the glass composition on the degradation and conversion of the scaffolds to a hydroxyapatite (HA)-type material in a simulated body fluid (SBF) are reported here (Part I). The in vitro response of osteogenic cells to the scaffolds and the in vivo evaluation of the scaffolds in a rat subcutaneous implantation model are described in Part II. Scaffolds (porosity = 78-82%; pore size = 100-500 microm) were prepared using a polymer foam replication technique. The glasses consisted of a silicate (13-93) composition, a borosilicate composition (designated 13-93B1), and a borate composition (13-93B3), in which one-third or all of the SiO2 content of 13-93 was replaced by B2O3, respectively. The conversion rate of the scaffolds to HA in the SBF increased markedly with the B2O3 content of the glass. Concurrently, the pH of the SBF also increased with the B2O3 content of the scaffolds. The compressive strengths of the as-prepared scaffolds (5-11 MPa) were in the upper range of values reported for trabecular bone, but they decreased markedly with immersion time in the SBF and with increasing B2O3 content of the glass. The results show that scaffolds with a wide range of bioactivity and degradation rate can be achieved by replacing varying amounts of SiO(2) in silicate bioactive glass with B2O3.
27
Larry L. Hench · Journal of the American Ceramic Society · 1998 · 2.6K citations
Handbook of Chemistry and Physics
M. Tobias · Nuclear Science and Engineering · 1961 · 1.4K citations