Optics Express · 2009 · 55 citations · 17 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMicrofabricationOpticsConfocal MicroscopyDamage MechanicsFracture MechanicsLaser Material ProcessingLaser OpticsLaser PhysicsBeam Pulse DurationConfocal Fluorescence MicroscopyConfocal Laser Scanning MicroscopyCracksFemtosecond Laser ParametersLaser Pulse DurationLaser-induced EffectsPulse Duration Effects
Significant improvement in the polishing process of fused silica optical components has increased their lifetimes at 351 nm. Nevertheless, for large laser facilities like the LaserMegaJoule (LMJ), zero defect optical components are not yet available. Therefore, a damage mitigation technique has been developed to prevent the growth of the laser-initiated damage sites. Because of the difficulty to produce mitigated sites with sufficiently large depth, the initial morphology of damage to mitigate is a critical issue. The aim of this work is to determine laser parameters (pulse duration, fluence) which permit us to initiate damage sites in accordance with our mitigation process. Confocal microscopy is used to observe damage sites that have sub-surface cracks and consequently to measure precisely the diameter and the depth of the area to mitigate.
17
National Ignition Facility laser performance status
C. Haynam, Paul J. Wegner, Jerome M. Auerbach et al. · Applied Optics · 2007 · 574 citations
Natural Sciences, Nuclear Engineering, Nuclear Instrumentation +15
The French Megajoule Laser Project (LMJ)
Michel André · Fusion Engineering and Design · 1999 · 113 citations
Growth of laser-initiated damage in fused silica at 351 nm
Mary A. Norton, Lawrence W. Hrubesh, Zhouling Wu et al. · Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE · 2001 · 80 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +11