Mineralogical Magazine · 1982 · 48 citations · 5 references
Natural SciencesChemistryCrystal StructureInorganic ChemistryMineralogyCrystal ChemistryCrystallization ProcessesMineral ChemistryMineral ClassificationMineral GeochemistryPhysical Properties Of MineralsAbsorption SpectrumMonoclinic SystemPowder DiffractionPowder Diffraction AnalysisPowder X-ray Diffraction
Abstract Euhedral crystals of the low-temperature mineral lansfordite, MgCO 3 · 5H 2 O, have been prepared from saturated magnesium bicarbonate solutions at temperatures below 10°C. The crystals are monoclinic P 2 1 / a with a = 12.4758(7), b = 7.6258(4), c = 7.3463(6)Å, β = 101.762(6)°, V = 684.24Å 3 , D calc. = 1.693 g cm −3 , D obs. = 1.70(1) g m −3 . At room temperature, the crystals slowly effloresce to produce pseudomorphs of nesquehonite, MgCO 3 · 3H 2 O. Dehydration is complete at 300°C, with decarbonation taking place in the interval to 560°C. A new X-ray powder diffraction pattern is presented, and details of the infra-red absorption spectrum are discussed.
5
The infrared spectra of minerals
Robert E. Newnham · Materials Research Bulletin · 1975 · 1K citations
Sedimentary carbonate minerals
Earth-Science Reviews · 1973 · 554 citations · Full text
The transformation of nesquehonite into hydromagnesite
Peter J. Davies, B. Bubela · Chemical Geology · 1973 · 236 citations