Japanese Journal of Applied Physics · 1989 · 19 citations · 7 references
Natural SciencesMaterials EngineeringMaterials ScienceCondensed Matter PhysicsPhase TransformationsSolid State PhysicsCrystallization ProcessesHigh-temperature MaterialsNucleationSuperconducting MaterialsCalcinationCuprate SuperconductorsHigh-temperature SuperconductivityHigh-temperature SuperconductorsSol-gel ProcessingSol-gel SystemsSuperconducting CeramicsX-ray Diffraction Analysis
An oxide superconductor in the Bi, Pb-Sr-Ca-Cu-O system has been prepared by the sol-gel method, and the effect of calcination temperature on the formation of the high- T c phase has been examined. Calcination at 830°C before the reheat treatment at 845°C is the most effective for the formation of the high- T c phase, as revealed by X-ray diffraction analysis. From this fact, we conclude that the nucleation of the high- T c phase is apt to take place at around 830°C. The T c value of the specimen calcined at 830°C and reheated at 845°C for 24 h is 90 K.
7
Sputter Deposition of BiSrCaCuO Thin Films
Masao Fukutomi, Junichi Machida, Yoshiaki Tanaka et al. · Japanese Journal of Applied Physics · 1988 · 692 citations