Superconducting films fabricated by high-fluence Ga implantation in Si

J. Fiedler, V. Heera, R. Skrotzki, T. Herrmannsdörfer, M. Voelskow, A. Mücklich, Steffen Oswald, B. Schmidt, W. Skorupa, G. Gobsch,

Physical Review B · 2011 · 21 citations · 34 references

Concepts

Abstract

Ga-rich layers in Si were fabricated by 80 keV Ga implantation through a 30 nm SiO${}_{2}$ cover layer and subsequent rapid thermal annealing for 60 s in a temperature range between 500 \ifmmode^\circ\else\textdegree\fi{}C and 1000 \ifmmode^\circ\else\textdegree\fi{}C. Fluences of 2\ifmmode\times\else\texttimes\fi{}10${}^{16}$ cm${}^{\ensuremath{-}2}$ and 4\ifmmode\times\else\texttimes\fi{}10${}^{16}$ cm${}^{\ensuremath{-}2}$, leading to Ga peak concentrations of 8 at. % and 16 at. %, are chosen. Residual damage in the implanted layers and the Ga distribution were investigated by Rutherford-backscattering spectrometry in combination with ion channeling, cross-sectional electron microscopy, and x-ray photoelectron spectroscopy. Temperature-dependent Hall-effect measurements were carried out in order to determine the electrical properties of the implanted layers. It is shown that annealing at temperatures up to 800 \ifmmode^\circ\else\textdegree\fi{}C leads to the formation of polycrystalline layers containing random distributed amorphous clusters. At the Si/SiO${}_{2}$ interface a dense and narrow band of Ga-rich clusters is observed. For 4 \ifmmode\times\else\texttimes\fi{} 10${}^{16}$ cm${}^{\ensuremath{-}2}$ the amount of mobile Ga is higher than for 2\ifmmode\times\else\texttimes\fi{}10${}^{16}$ cm${}^{\ensuremath{-}2}$ and an increase of the cluster density at the Si/SiO${}_{2}$ interface was found. Due to the higher cluster density for 4\ifmmode\times\else\texttimes\fi{}10${}^{16}$ cm${}^{\ensuremath{-}2}$ this interface layer can become superconducting below 7 K with critical fields exceeding 9 T at optimized annealing conditions. Critical currents are above 1 kA/cm${}^{2}$ and therefore this seems to be a possible material system for future microelectronic applications. After annealing at 900 \ifmmode^\circ\else\textdegree\fi{}C and above, the implanted layers are single crystalline and no amorphous precipitates were detected.

References

34