Nanometer-Sized Zeolite X Crystals:  Use as Photochemical Hosts

Norma B. Castagnola, Prabir K. Dutta

The Journal of Physical Chemistry B · 1998 · 85 citations · 34 references

Concepts

Abstract

A patent procedure was followed to synthesize 250 nm aggregates of individual 13 ± 2.5 nm crystallites of zeolite X. A low-temperature aging step and addition of sucrose to the reaction mixture were required to get optimum quality of crystals. Conventional ship-in-a-bottle synthesis of Ru(bpy) 3 2+ in the cages of these nanocrystallites resulted in considerable framework degradation, with only 10% of the crystallinity in the original crystals being retained. The degradation occurred due to exposure to mild acidity and thermal treatment during synthesis of Ru(bpy) 3 2+ . The procedure was modified to avoid acidity in the initial ion-exchange step of Ru(NH 3 ) 6 3+, resulting in a Ru(bpy) 3 2+ −zeolite with 75% of the crystallinity retained. Acidity generated during conversion of Ru(NH 3 ) 6 3+ to Ru(bpy) 3 2+ was thought to be responsible for the degradation. A third procedure starting with the highly air-sensitive Ru(NH 3 ) 6 2+ resulted in formation of Ru(bpy) 3 2+ −zeolite with about 90% crystallinity. In all three procedures, the Ru(bpy) 3 2+ molecules were entrapped within the framework. Ion exchange of viologen molecules and the fluorescence quenching of photoexcited Ru(bpy) 3 2+ by intrazeolitic viologen increased with the increase of zeolite crystallinity. Interfacial zeolite−solution electron transfer upon visible light photoexcitation of the Ru(bpy) 3 2+ −zeolite−viologen system demonstrated an increase in permanent charge separation efficiency as the crystallinity of the zeolite is preserved. Because of the higher surface-to-volume ratios, the charge separation efficiency in the nanocrystallites was a factor of 2 better than conventional micron-sized zeolite Y crystallites under identical photolysis conditions.

References

34