physica status solidi (a) · 1995 · 18 citations · 8 references
Natural SciencesMaterials EngineeringMaterials ScienceCrystal StructureInorganic ChemistrySolid-state ChemistryCrystal ChemistryCrystal GrowthCrystallization ProcessesCrystal Growth KineticsCrystal Growth MechanismsCrystal Growth ThermodynamicsLow-temperature GrowthOptimum TemperatureTemperature Optimum
Bi2Sr2CaCu2Oy single crystals are prepared by a self-flux method using the crucible with a cap. From the results, it is found that the optimum cooling rate and the optimum temperature ending the growth are 1 K/h and 830°C, respectively. A plate-like Bi2Sr2CaCu2Oy single crystal with the size of 6 × 2 mm2 is obtained which is 80 K single-phase.
8
Superconductivity in the Bi-Sr-Cu-O System
Jun Akimitsu, Akira Yamazaki, Hiroshi Sawa et al. · Japanese Journal of Applied Physics · 1987 · 372 citations