HIGH RESISTANCE ANODIC OXIDE FILMS ON ALUMINIUM

A. C. Harkness, L. Young

Canadian Journal of Chemistry · 1966 · 153 citations · 7 references

Concepts

Abstract

The thicknesses of oxide films formed in aqueous borate solutions were obtained by the spectrophotometric method after developing the interference colors by evaporating a very thin film of gold or bismuth onto the oxide. The refractive index of the stripped films was determined by the Becke immersion method as 1.57 to 1.58 at 5 900 Å wavelength. The dielectric constant was estimated as 9.8 ± 0.5. Experimental data on the steady state ionic current density, I, through the oxide as a function of the field strength, E, in the oxide could be represented by I = I 0 exp −(W − qaE)/kT where I 0 = 2.24 × 10 7 A cm −2 , W = 1.3 ± 0.15 eV, q = 3e, a = 2.95 ± 0.15 Å.

References

7