Deposition of MBa<sub>2</sub>Cu<sub>3</sub>O<sub>7-x</sub>thin films by channel-spark method

Violeta Dediu, Q D Jiang, F.C. Matacotta, Paolo Scardi, Marco Lazzarino, G. Nieva, L. Civale

Superconductor Science and Technology · 1995 · 40 citations · 8 references

Concepts

Abstract

Channel-spark pulsed electron beam deposition (CS), a new deposition method based on a simple and inexpensive system, has been used for preparation of high-quality GdBa2Cu3O7-x, Gd1-xEuxBa2Cu3O7-x and YBa2Cu3O7-x thin films epitaxially grown on NdGaO3 and SrTiO3 substrates. Typical critical temperatures for zero DC resistance lie in the intervals 87-89 K for Y-based films and 91.0-92.6 K for Gd- and GdEu-based ones. The transition widths for the best films are less than 0.5 K. The critical current densities reach the values of 3*106 A cm-2 at 77 K, zero field.

References

8