Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsMicroelectromechanical SystemsThin FilmsDielectricsFerroelectric CeramicsFerroelectric MaterialsPiezoelectric MaterialsThin Film Mechanical PropertiesThin-film MaterialsDielectric ConstantMagnetron SputteringMorphotropic Phase BoundaryPiezoelectric PropertiesPiezoelectric Thin FilmsTetragonal AxesThin Oxide FilmsThin-film Piezoelectrics
The c -axis oriented Pb(Zr, Ti)O 3 (PZT) thin films, which have a tetragonal structure and a composition near the morphotropic phase boundary, have been obtained on (100)MgO substrates with (100)Pt electrodes by rf-magnetron sputtering. These PZT thin films have a remarkably low relative dielectric constant of 240. The intrinsic piezoelectric and mechanical properties of the thin films were evaluated. The velocity of sound and the mechanical compliance s 11 E were measured by the piezoelectric resonance of the cantilever. The piezoelectric coefficient d 31 was measured directly from the transverse expansion of the cantilever beams. Even without a poling treatment, d 31 of the PZT thin films was -100 pC/N and almost the same as that of bulk ceramics. The extremely large piezoelectric coefficient g 31 of -57×10 -3 Vm/N was also estimated because of the large d 31 and remarkably low dielectric constant. These PZT thin films are suitable for micro sensor and actuator applications.
11
Piezoelectric properties of c-axis oriented Pb(Zr,Ti)O3 thin films
Isaku Kanno, Satoru Fujii, Takeshi Kamada et al. · Applied Physics Letters · 1997 · 252 citations
Natural Sciences, Materials Engineering, Materials Science +17