Grain boundary properties of TlBa<sub>2</sub>Ca<sub>2</sub>Cu<sub>3</sub>O<sub>x</sub>and Tl<sub>2</sub>Ba<sub>2</sub>CaCu<sub>2</sub>O<sub>x</sub>thin films

H. Suhara, Toshihide Nabatame, O.B. Hyun, S. Koike, I. Hirabayashi

Superconductor Science and Technology · 1995 · 18 citations · 21 references

Concepts

Abstract

We have investigated the transport properties of the grain boundaries of TlBa2Ca2Cu3Ox (Tl-1223) and Tl2Ba2CaCu2Ox (Tl-2212) epitaxial thin films. Both Tl-1223 and Tl-2212 thin films were grown on SrTiO3 bicrystal substrates with various tilt angles (5 degrees , 10 degrees , 15 degrees , 24 degrees and 36.8 degrees ) of (001) direction by a laser ablation and post-annealing method. For both Tl-1223 and Tl-2212 phases, the grain boundary Jc for large tilt angles ( theta >or=15 degrees ) at 5 K dropped by almost one order of magnitude, compared with the intragrain Jc. We also observed hysteretic magnetic-field dependence of grain boundary Jc for large tilt angles in both phases. On the other hand, the grain boundaries for low tilt angles ( theta <or=10 degrees ) retained high Jc in low magnetic fields. The critical tilt angle was found to have the same value (10 degrees ) in both phases and greater than that ( theta approximately=5 degrees ) for the YBa2Cu3O7- delta system. These results suggest that the grain boundaries for high tilt angle larger than 15 degrees limit transport critical current density as weak links for Tl-Ba-Ca-Cu-O systems.

References

21