Journal of The Electrochemical Society · 1968 · 43 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceMetallurgyPhysical ChemistrySurface ScienceAlloysFerrous MetallurgyHigh-temperature OxidationIron OxidesMetalsSurface OxidationActivation EnergyElectron Probe MicroanalysisMicroanalysisOxidationOxidation KineticsOxide Scale FormationOxide Scale GrowthScale Formation Kinetics
, containing small quantities of dissolved iron, is the only oxide formed in the oxidation of iron‐chromium alloys in the range 22–68% Cr in oxygen at 800°–1200°C; it is also formed, at least initially, on alloys containing 14 and 18% Cr. The oxide growth is diffusion‐controlled, with an apparent activation energy of 36 kcal mole−1. The increase in oxidation rate with alloy chromium content is slight up to 37% Cr, but becomes more marked with the chromium‐rich alloys. Iron only enters the scale during the very early stages of oxidation, so the weight fraction of iron in the oxide decreases with time. Alloy interdiffusion coefficients have been determined from chromium concentration profiles in the underlying alloy. The activation energies for inter‐ diffusion are 51 and 59 kcal mole−1 for Fe‐27% Cr and Fe‐59% Cr, respectively, but interdiffusion is much slower for the chromium‐rich alloy. The chromium concentration at the alloy/oxide interface, which is determined largely by the ratio of oxidation rate to alloy interdiffusion rate, governs the type of oxide formed if lifting and cracking of the stressed scale occurs. Factors affecting the tendency for scale failure in this way are discussed.