TechnoRep (University of Belgrade – Faculty of Technology and Metallurgy) · 2014 · 10 citations · 17 references
EngineeringMaterials EngineeringMaterials ScienceMaterials ProcessingMechanical Behavior Of MaterialsMetallurgyExtractive MetallurgyFerrous MetallurgyMechanical CharacterizationPowder MetallurgyPowder ProcessingPowder TechnologyActivationEnergy ConsumptionGrindingMilling TechnologyPowder CharacterizationProcess ParametersSpecific EnergySpecific Energy Consumption
The efficiency of talc mechanical activation by means of two different mechano-activators centrifugal and attrition mill is investigated in this study and the comparative analysis of the characteristics of obtained talc powders is presented. A new approach for obtaining high-grade talc concentrate with low Fe2O3 content is achieved through effect of mechanical activation of talc accompanied by hydrometallurgical process. The applied mechanical activation process conditions of ultra-centrifugal mill were defined by number of rotor revolutions, sieve mesh size, and current intensity. These operating parameters of the ultra-centrifugal mill were variable. Ultra fine grinding of talc in attrition mill (attritor) was carried out in various time intervals - from 5 to 15 min. The following technological parameters of the mechanical activation were monitored: time of mechanical activation, circumferential rotor speed, capacity of ultra-centrifugal mill, and specific energy consumption. The investigation was based on a kinetic model. The structure and behavior of activated samples were characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD) analysis, and differential thermal analysis (DTA).
17