Bulletin of the Korean Chemical Society · 2003 · 46 citations · 7 references
Natural SciencesChemical EngineeringChemistryCatalysisInorganic ChemistryReaction EngineeringCatalyst CharacterizationCatalyst DeactivationCatalyst StabilityCatalytic MaterialsCatalytic Reaction EngineeringRedox CatalysisAlumina CatalysisCatalyst MechanismsMetal Oxide CatalystsMetal Oxide NanocatalystsSelectivityStability Under Reaction ConditionsStability-selectivity RelationshipsWater-gas Shift Reaction
Reverse-Water-Gas-Shift reaction (RWGSR) was carried out over the ZnO, <TEX>$Al_2O_3,\;and\;ZnO/Al_2O_3$</TEX> catalysts at the temperature range from 400 to 700 ℃. The ZnO showed good specific reaction activity but this catalyst was deactivated. All the catalysts except the <TEX>$ZnO/Al_2O_3$</TEX> catalyst (850 ℃) showed low stability for the RWGSR and was deactivated at the reaction temperature of 600 ℃. The <TEX>$ZnO/Al_2O_3$</TEX> catalyst calcined at 850 ℃ was stable during 210 hrs under the reaction conditions of 600 ℃ and 150,000 GHSV, showing CO selectivity of 100% even at the pressure of 5 atm. The high stability of the <TEX>$ZnO/Al_2O_3$</TEX> catalyst (850 ℃) was attributed to the prevention of ZnO reduction by the formation of <TEX>$ZnAl_2O_4$</TEX> spinel structure. The spinel structure of <TEX>$ZnAl_2O_4$</TEX> phase in the <TEX>$ZnO/Al_2O_3$</TEX> catalyst calcined at 850 ℃ was confirmed by XRD and electron diffraction.
7
Sang-Woo Park, Oh‐Shim Joo, Kwang‐Deog Jung et al. · Applied Catalysis A General · 2001 · 146 citations