EngineeringMaterials EngineeringMaterials ScienceCeramic MaterialsMetallic MaterialsMetallurgyAlloysCastingFerrous MetallurgyMagnetic Properties Of SolidsMetal CastingPhysical MetallurgyCasting AlloysCoercivityCoercivity EnhancementCooling Rate EffectsMagnetic CoercivityNanocrystalline AlloysNanocrystalline CeramicsQuenched Phases
The structure and the coercivity (Hc) of rapidly quenched (Fe0.55Pt0.45)bal.Zr0–8B0–24 alloys prepared by the melt-spinning technique have been investigated. Ordered L10 Fe–Pt phase of 20–100 nm was obtained by rapidly quenching the melt for (Fe0.55Pt0.45)78Zr2B20 and (Fe0.55Pt0.45)78Zr4B18 alloys with high Hc of 341 and 649 kA/m in an as-quenched state, respectively. On the other hand, the (Fe0.55Pt0.45)78Zr4B18 alloy produced by Cu mold casting at a lower cooling rate than melt spinning is found to be composed of a mixed structure of Fe–Pt L10, ZrB12, PtZr and Fe3B phases and the alloy has much lower Hc of 74 kA/m than that of the melt-spun (Fe0.55Pt0.45)78Zr4B18 alloy. The lattice parameters (a and c) of the L10 phase in the melt-spun alloys suggest that Zr and B elements are contained in the L10 phase for the melt-spun alloys, which is possibly related to direct formation of the L10 structure by rapidly quenching the melt.
12
Monodisperse FePt Nanoparticles and Ferromagnetic FePt Nanocrystal Superlattices
Shouheng Sun, C. B. Murray, D. Weller et al. · Science · 2000 · 6.1K citations