2006 · 13 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsMetallurgyCorrosion EngineeringCorrosion MechanismsCorrosion Of SteelsCorrosion TestingStainless SteelsStress Corrosion CrackingAustenitic Stainless Steel CorrosionAustenitic Stainless SteelsAustenitic SteelsOperational LimitsPitting Corrosion TestingStainless Steel CorrosionStress Corrosion Cracking AssessmentStress Corrosion Cracking Testing
Abstract This paper describes a series of tests on two grades of stainless steels UNS S31600 (AISI 316) and UNS S66286 (ASTM A453 Gr. 660– Alloy A286) in simulated H2S-contining oil and gas service environments. The purpose of this study was to evaluate these materials for stress corrosion cracking. Triplicate, stressed C-ring specimens of each material were exposed to a 5% NaCl and 0.4% NaCH3COO solution equilibrated with a 1.5 psia (10.3 kPa) H2S at 200 F (93 C), 250 F (121 C) and 300 F (149 C) for 30 days. After exposure, none of the C-rings showed signs of cracking. The UNS S31600 specimens did exhibit pitting after testing at all three temperatures. None of the UNS S66286 (A286) C-rings exhibited pitting after exposure. Following this initial effort, additional tests at 300 F (149 C) were performed consisting of triplicate specimens immersed in three different solutions saturated with 15 psia (103 kPa) H2S: (a) 5% NaCl solution with a pH of 5.5, (b) 16% NaCl solution with a pH of 5.5, and (c) 5% NaCl solution with a pH of 4.5. After these exposures, none of the C-rings immersed in the 5% NaCl solution with a 5.5 pH showed signs of cracking. Two UNS S31600 and one UNS S66286 specimens failed after exposure to the 16% NaCl solution with a pH of 5.5. In addition, one UNS S31600 all three UNS S66286 specimens failed after testing in the 16% NaCl solution with a pH of 4.5. Several of the UNS S31600 specimens exhibited pitting after testing. The maximum pit depth was 10.2 mils (0.26 mm) on a UNS S31600 specimen exposed to the 16% NaCl / pH 5.5 environment. None of the UNS S66286 exhibited pitting after exposure.