Bioactive Materials · 2024 · 10 citations · 49 references
MedicineOrthopedic SurgeryBiomechanicsOrthopaedic BiomaterialsOrthopedic BiomaterialsBiomechanical InstrumentationFixation BiomechanicsImplant BiomechanicsImplant MaterialsBiomechanical Testing Of ImplantsFracture Fixation DevicesImplant Condition AssessmentImplantable SensorsImplantable Temperature SensorsMagnesium-based ImplantsMechanical LoadingMechanical Properties Of Implants
Biodegradable magnesium is a highly desired material for fracture fixation implants because of its good mechanical properties and ability to completely dissolve in the body over time, eliminating the need for a secondary surgery to remove the implant. Despite extensive research on these materials, there remains a dearth of information regarding critical factors that affect implant performance in clinical applications, such as the in vivo pH and mechanical loading conditions. We developed a measurement system with implantable strain, temperature, pH and motion sensors to characterize magnesium and titanium plates, fixating bilateral zygomatic arch osteotomies in three Swiss alpine sheep for eight weeks. pH 1–2 mm above titanium plates was 6.6 ± 0.4, while for magnesium plates it was slightly elevated to 7.4 ± 0.8. Strains on magnesium plates were higher than on titanium plates, possibly due to the lower Young's modulus of magnesium. One magnesium plate experienced excessive loading, which led to plate failure within 31 h. This is, to our knowledge, the first in vivo strain, temperature, and pH data recorded for magnesium implants used for fracture fixation. These results provide insight into magnesium degradation and its influence on the in vivo environment, and may help to improve material and implant design for future clinical applications. • We designed a custom embedded system to measure strain, temperature and pH in vivo . • Data was recorded from Ti and resorbable Mg plates fixating ovine zygoma osteotomies. • No initial pH increase near PEO-coated Mg plates; pH decreases near osteotomized bone. • In vivo strains were measured bidirectionally during normal activity. • Plate placement significantly affects in vivo strains and can lead to early failure.
49
A survey of bio-corrosion rates of magnesium alloys
Nicholas Travis Kirkland, J. Lespagnol, N. Birbilis et al. · Corrosion Science · 2009 · 483 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +14
Characterization of parylene C as an encapsulation material for implanted neural prostheses
Christina Hassler, Rene P. von Metzen, Patrick Ruther et al. · Journal of Biomedical Materials Research Part B Applied Biomaterials · 2010 · 262 citations
Natural Sciences, Materials Engineering, Materials Science +15