Effect of multiple firings on optical and mechanical properties of Virgilite-containing lithium disilicate glass-ceramic of varying thickness

Amr Rizk, Ahmed Abdou, Reem Ashraf, Sarah Omar

Clinical Oral Investigations · 2024 · 12 citations · 27 references

DOIFull text

Open access

Concepts

Abstract

Abstract Objectives To investigate the effect of multiple firings on color, translucency, and biaxial flexure strength of Virgilite-containing (Li 0.5 Al 0.5 Si 2.5 O 6 ) lithium disilicate glass ceramics of varying thickness. Materials and methods Sixty discs were prepared from Virgilite-containing lithium disilicate blocks. Discs were divided according to thickness ( n = 30) into T 0.5 (0.5 mm) and T 1.0 (1.0 mm). Each thickness was divided according to the number of firing cycles ( n = 10); F 1 (Control group): 1 firing cycle; F 3 : 3 firing cycles, and F 5 : 5 firing cycles. The discs were tested for color change (ΔE 00 ) and translucency (TP 00 ) using a spectrophotometer. Then, all samples were subjected to biaxial flexure strength testing using a universal testing machine. Data were collected and statistically analyzed (α = 0.5). For chemical analysis, six additional T 0.5 discs (2 for each firing cycle) were prepared; for each firing cycle one disc was subjected to X-ray diffraction analysis (XRD) and another disc was subjected to Energy dispersive X-ray spectroscopy (EDX) and Scanning electron microscope (SEM). Results Repeated firing significantly reduced the translucency of F 3 and F 5 compared to F 1 in T 0.5 ( p < 0.001), while for T 1.0 only F 5 showed a significant decrease in TP 00 ( p < 0.001). For ΔE 00 , a significant increase was recorded with repeated firings ( p < 0.05) while a significant decrease resulted in the biaxial flexure strength regardless of thickness. Conclusions Repeated firings had a negative effect on both the optical and mechanical properties of the Virgilite-containing lithium disilicate glass ceramics. Clinical relevance Repeated firings should be avoided with Virgilite-containing lithium disilicate ceramics to decrease fracture liability and preserve restoration esthetics.

References

27