Construction and Building Materials · 2024 · 18 citations · 38 references
Natural SciencesMaterials EngineeringMaterials ScienceBuilding MaterialsCeramic MaterialsMechanical Behavior Of MaterialsBrick UnitsFire TestingFire-resistant MaterialsHigh-temperature MaterialsMaterial PropertiesCeramic Tile MaterialsCompressive StrengthCompressive Strength DevelopmentDemolition WasteElevated-temperature Material PropertiesFire-induced Structural FailureMaterial Behaviour At Elevated TemperaturesMicrostructural Degradation
The mechanical behavior of materials based on the alkali activation of construction and demolition waste during and after their exposure to high temperatures was studied. The studied materials were based entirely on either, waste bricks or waste ceramic tiles, while a potassium hydroxide / sodium silicate solution was used as alkali activator. The compressive deformation of the alkali activated materials was tested during exposure to 850 - 1050 °C (on-fire testing) and the residual compressive strength was measured after exposure to 600 - 1050 °C for 2 h (post-fire testing), simulating the standard ISO 834 time-temperature curve. Microstructural changes and bulk properties were also assessed. The experimental results showed similar behavior of both materials in post-fire tests. Their compressive strength declined in between 600 and 800 °C and rose at 1050 °C, exceeding the initial value. Their density decreased 8 - 9% at 1050 °C, while their mass loss was 7 - 10% at this temperature. In the on-fire tests, the waste ceramic tile-based material presented plastic strain without any obvious macro-fracture at all the temperatures tested, while the waste brick-based material retained its elasticity and behaved as ceramic material up to 1000 °C with obvious macro-fractures. According to the experimental results, both alkali activated materials have the potential to be used as fire-resistant building materials.
38
Geopolymer technology: the current state of the art
Peter Duxson, A. Fernández‐Jiménez, John L. Provis et al. · Journal of Materials Science · 2006 · 4.5K citations
Effect of synthesis parameters on the mechanical properties of fly ash-based geopolymers
Dimitrios Panias, Ioanna Giannopoulou, Theodora Perraki · Colloids and Surfaces A Physicochemical and Engineering Aspects · 2006 · 718 citations · Full text